Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.115 GPa @Temperature 120 °C |
16.7 ksi @Temperature 248 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |