Polymer Property : Shear Strength = 9200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 63.4 MPa

@Temperature 149 °C
9200 psi

@Temperature 300 °F
Short Beam
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber
Information provided by HexCel