Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 6.30 MPa @Temperature 22.0 °C |
914 psi @Temperature 71.6 °F |
Short Beam Shear; Dry; 30 min @ 150°C; DMS2180 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |
|||
Shear Strength | 6.30 MPa @Temperature 22.0 °C |
914 psi @Temperature 71.6 °F |
Short Beam Shear; Dry; 20 min @ 175°C; DMS2180 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |