Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 88.3 MPa @Temperature 121 °C |
12800 psi @Temperature 250 °F |
In-Plane, Dry, 365° Oven Cured; ASTM D3518 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Shear Strength | 88.3 MPa @Temperature 177 °C |
12800 psi @Temperature 351 °F |
Short Beam; Autoclave Cured; [0°]16 |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |