Polymer Property : Shear Strength = 86.05 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 86.05 MPa

@Temperature 22.8 °C
12480 psi

@Temperature 73.0 °F
ILSS Long; 10 min @ 250°F
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle
Information provided by HexCel
Shear Strength 86.05 MPa

@Temperature 22.8 °C
12480 psi

@Temperature 73.0 °F
ILSS Long; 30 min @ 250°F
Hexcel® HexPly® EF01 Epoxy Curing System after THR 120 EF01 S25 38% Curing Cycle