Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 58.6 MPa @Temperature 23.9 °C |
8500 psi @Temperature 75.0 °F |
Short Beam; Dry; ASTM D2344 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Shear Strength | 58.6 MPa @Temperature 90.6 °C |
8500 psi @Temperature 195 °F |
0° Short Beam, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Shear Strength | 58.6 MPa @Temperature 90.6 °C |
8500 psi @Temperature 195 °F |
Fill Short Beam, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Shear Strength | 58.6 MPa @Temperature 163 °C |
8500 psi @Temperature 325 °F |
Short Beam |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |