Mechanical Properties Metric English Comments
Shear Strength 85.5 MPa

@Temperature 23.0 °C
12400 psi

@Temperature 73.4 °F
ASTM D732
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications. Torlon PAI has the highest..
Shear Strength 85.5 MPa

@Temperature 23.0 °C
12400 psi

@Temperature 73.4 °F
ASTM D732
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)
Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda..