Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 84.8 MPa @Temperature 82.0 °C |
12300 psi @Temperature 180 °F |
Short Beam, Dry |
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber Information provided by HexCel |