Shear Strength 5.58 MPa

@Temperature 82.0 °C
810 psi

@Temperature 180 °F
Overlap, FRP
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Shear Strength 5.58 MPa

@Temperature 24.0 °C
810 psi

@Temperature 75.2 °F
Overlap, ABS
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 5.58 MPa

@Temperature 24.0 °C
810 psi

@Temperature 75.2 °F
Overlap, ABS
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 5.58 MPa

@Temperature 24.0 °C
810 psi

@Temperature 75.2 °F
Overlap, ABS
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..