Mechanical Properties Metric English Comments
Shear Strength 81.4 MPa

@Temperature 177 °C
11800 psi

@Temperature 350 °F
In-plane, Dry; SACMA SRM 7R-94
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric
MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties ..
Shear Strength 81.4 MPa

@Temperature 23.0 °C
11800 psi

@Temperature 73.4 °F
JIS K7214
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Shear Strength 81.4 MPa

@Temperature 23.0 °C
11800 psi

@Temperature 73.4 °F
JIS K7214
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Shear Strength 81.4 MPa

@Temperature 25.0 °C
11800 psi

@Temperature 77.0 °F
Fill Short Beam, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel