Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.62 MPa @Temperature 23.0 °C |
1250 psi @Temperature 73.4 °F |
Overlap, Polyacrylic, Substrate Failure |
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 8.62 MPa @Temperature 23.0 °C |
1250 psi @Temperature 73.4 °F |
Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |