Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 49.6 MPa @Temperature 23.0 °C |
7190 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% VoidsInformation provided by HexCel |
|||
Shear Strength | 49.6 MPa @Temperature 177 °C |
7190 psi @Temperature 351 °F |
Short Beam |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |
|||
Shear Strength | 49.6 MPa @Temperature 177 °C |
7190 psi @Temperature 351 °F |
Short Beam, Wet |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |
|||
Shear Strength | 49.6 MPa @Temperature 177 °C |
7190 psi @Temperature 351 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel |