Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 48.3 MPa @Temperature 149 °C |
7010 psi @Temperature 300 °F |
Short Beam, Wet |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |