Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 43.5 MPa @Temperature -55.0 °C |
6310 psi @Temperature -67.0 °F |
Adhered: 50 MIL (17-7 Stainless Steel), Adhesive AF-126 (0.06 wt) |
3M Scotch-Weld™ 3901 Metal Primer 3M™ Scotch-Weld™ Metal Primer 3901 is a primer for 3M™ Scotch-Weld™ film and liquid adhesives in those applications where it is desired to obtain improved metal and glass adhesion or improved re.. |