Polymer Property : Shear Strength = 6.65 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 6.65 MPa

@Temperature -34.0 °C,
Time 1.81e+6 sec
964 psi

@Temperature -29.2 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..
Shear Strength 6.65 MPa

@Temperature -34.0 °C,
Time 1.81e+6 sec
964 psi

@Temperature -29.2 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..