Mechanical Properties Metric English Comments
Shear Strength 6.62 MPa

@Temperature 21.1 °C
960 psi

@Temperature 70.0 °F
Double Lap Shear (Composite/Composite), 0.05 psf, No conditioning
Hexcel® Redux® 330K Epoxy film adhesives for the bonding and finishing of composites
Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl..
Shear Strength 6.62 MPa

@Temperature 0.000 °C
960 psi

@Temperature 32.0 °F
Tensile, Al/Al lap joint; cured 7 days @ 25°C
Abatron AboCast 8110-4/AboCure 8110-3 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Shear Strength 6.62 MPa

@Temperature 24.0 °C
960 psi

@Temperature 75.2 °F
Overlap, Rigid PVC
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 6.62 MPa

@Temperature 24.0 °C
960 psi

@Temperature 75.2 °F
Overlap, Rigid PVC
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 6.62 MPa

@Temperature 24.0 °C
960 psi

@Temperature 75.2 °F
Overlap, Rigid PVC
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..