Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 6.21 MPa @Temperature 177 °C |
900 psi @Temperature 351 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Sc.. |