Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 36.5 MPa @Temperature 71.1 °C |
5300 psi @Temperature 160 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |