Mechanical Properties Metric English Comments
Shear Strength 34.5 MPa

@Temperature 21.1 °C
5000 psi

@Temperature 70.0 °F
2 hrs @ 250°F, Metal Clamp Pressure, 6061 T6 FPL Etched
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive
Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe..
Shear Strength 34.5 MPa

@Temperature 21.1 °C
5000 psi

@Temperature 70.0 °F
Lap Shear, Cured at 250°C for 60 min at 30 psi MMM-A-132 and MIL-A-25463.
Hexcel® Redux® 382H (0.06 psf) Film Adhesive
Redux 382H is a 250°F curing modified epoxy film adhesive available in both supported and unsupported versions. Redux 382H is a versatile adhesive system suitable for bonding a wide variety of subs..
Shear Strength 34.5 MPa

@Temperature 24.0 °C
5000 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ 2086 One-Part Epoxy Adhesives and Metal Primer
High Temperature strength and High ViscosityInformation provided by 3M
Shear Strength 34.5 MPa

@Temperature 82.0 °C
5000 psi

@Temperature 180 °F
Overlap
3M Scotch-Weld™ 2086 One-Part Epoxy Adhesives and Metal Primer
High Temperature strength and High ViscosityInformation provided by 3M
Shear Strength 34.5 MPa

@Temperature 24.0 °C
5000 psi

@Temperature 75.2 °F
with Scotch-Weld EW-5000; ASTM D1002-10
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive
3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion..
Shear Strength 34.5 MPa

@Temperature 24.0 °C
5000 psi

@Temperature 75.2 °F
No Primer; ASTM D1002-10
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive
3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion..