Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.345 MPa @Temperature 82.0 °C |
50.0 psi @Temperature 180 °F |
Overlap, 1/8 birch to 1/8 birch, bond tested after aging 3 weeks @ 24°C and 50% RH at a separation rate of 0.2 in/min; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 0.345 MPa @Temperature 82.0 °C |
50.0 psi @Temperature 180 °F |
1/8" Birch/High-Pressure Laminate, aged 9 mo |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Shear Strength | 0.345 MPa @Temperature 82.0 °C |
50.0 psi @Temperature 180 °F |
1/8" Birch/High-Pressure Laminate, aged 9 mo |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |