Polymer Property : Shear Strength = 5.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 5.00 MPa

@Temperature -55.0 °C
725 psi

@Temperature -67.0 °F
Beam Shear, No conditioning
Hexcel® Redux® 330M Epoxy film adhesives for the bonding and finishing of composites
Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl..
Shear Strength 5.00 MPa

@Temperature 21.1 °C
725 psi

@Temperature 70.0 °F
Beam Shear, No conditioning
Hexcel® Redux® 330M Epoxy film adhesives for the bonding and finishing of composites
Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl..
Shear Strength 5.00 MPa

@Temperature 71.1 °C
725 psi

@Temperature 160 °F
Beam Shear, No conditioning
Hexcel® Redux® 330M Epoxy film adhesives for the bonding and finishing of composites
Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl..