Mechanical Properties Metric English Comments
Shear Strength 33.8 MPa

@Temperature 71.1 °C
4900 psi

@Temperature 160 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Shear Strength 33.8 MPa

@Temperature 21.1 °C
4900 psi

@Temperature 70.0 °F
Lap Shear, Cured at 250°C for 60 min at 30 psi MMM-A-132 and MIL-A-25463, Exposure: 30 days salt spray.
Hexcel® Redux® 382H (0.06 psf) Film Adhesive
Redux 382H is a 250°F curing modified epoxy film adhesive available in both supported and unsupported versions. Redux 382H is a versatile adhesive system suitable for bonding a wide variety of subs..
Shear Strength 33.8 MPa

@Temperature 21.1 °C
4900 psi

@Temperature 70.0 °F
Lap Shear
Hexcel® Redux® 335M Adhesive film for bonding metallic and composite components (0.03 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..