Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 49.0 MPa

@Temperature 120 °C
7110 psi

@Temperature 248 °F
ILSS; prEN2563
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G803/1200 Fabric
Fiber: T300 3K, 285 g/m2Information provided by HexCel