Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 414 MPa @Strain 0.200 %, Thickness <=44.5 mm |
60000 psi @Strain 0.200 %, Thickness <=1.75 in |
|
Crucible Steel Aquamet® 18 Stainless Steel AQUAMET 18 is an austenitic stainless steel with corrosion resistance comparable to that of Type 304. Its good strength and toughness make it an ideal shafting material for workboats. It provides a .. |