Polymer Property : Shear Strength = 41.12 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.2835 MPa

@Shear Rate 5000 1/s,
Temperature 290 °C
41.12 psi

@Shear Rate 5000 1/s,
Temperature 554 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers