Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 23.0 MPa @Temperature 24.0 °C |
3340 psi @Temperature 75.2 °F |
Interlaminar |
Hexcel® HexPly® F263 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F263; Fiber: 75-1/0Information provided by HexCel |
|||
Shear Strength | 23.0 MPa @Temperature 132 °C |
3340 psi @Temperature 270 °F |
Short Beam |
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel |