Polymer Property : Shear Strength = 28.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 28.0 MPa

@Temperature 50.0 °C
4060 psi

@Temperature 122 °F
Lap Shear
Hexcel® Redux® 610W (0.03 psf) Flame retarded epoxy film adhesive
Redux 610 is a modified, flame-retarded epoxy film adhesive curing at 250°F. It is suitable for bonding metal to metal and for sandwich structures where flame retardancy and low heat release are re..