Polymer Property : Shear Strength = 23700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 163 MPa

@Temperature -53.9 °C
23700 psi

@Temperature -65.0 °F
Beam, V-Notched; Dry; Vacuum/Oven Cured; ASTM D5379-93
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...