Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 23.90 MPa @Temperature -55.0 °C |
3466 psi @Temperature -67.0 °F |
Tensile Lap Shear, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-1 |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |