Mechanical Properties Metric English Comments
Shear Strength 148 MPa

@Temperature 260 °C
21500 psi

@Temperature 500 °F
18-8 Stainless Steel butt joint
Lucas-Milhaupt BRAZE 541 Silver Based Cadmium Free Filler Metal
Characteristics:Braze 541 is an intermediate temperature silver brazing alloy with a rather long, 235EF (130EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting ..