Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.28 MPa @Temperature -40.0 °C |
330 psi @Temperature -40.0 °F |
Overlap, Polystyrene |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.28 MPa @Temperature -40.0 °C |
330 psi @Temperature -40.0 °F |
Overlap, Polystyrene |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 2.28 MPa @Temperature -40.0 °C |
330 psi @Temperature -40.0 °F |
Overlap, Polystyrene |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |