Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.31 MPa @Time 5400 sec |
190 psi @Time 1.50 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 1.31 MPa @Time 7200 sec |
190 psi @Time 2.00 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002 |