Polymer Property : Shear Strength = 18300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 126 MPa

@Temperature 25.0 °C
18300 psi

@Temperature 77.0 °F
+/- 45° In-Plane, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber
Information provided by HexCel