Mechanical Properties Metric English Comments
Shear Strength 0.0975 MPa

@Shear Rate 500 1/s,
Temperature 295 °C
14.1 psi

@Shear Rate 500 1/s,
Temperature 563 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..