Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 14.0 MPa @Temperature 177 °C |
2030 psi @Temperature 351 °F |
Short Beam |
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel |
|||
Shear Strength | 14.0 MPa @Temperature 177 °C |
2030 psi @Temperature 350 °F |
Lap Shear |
Hexcel® Redux® 641K Modified epoxy film adhesive for bonding metallic and composite components Redux 641 is a high temperature modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures where operating temperatures are experienced up t.. |