Polymer Property : Shear Strength = 135 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
Short Beam; Autoclave Cured; [0°]16
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form
Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel