Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 88.9 MPa @Temperature 23.9 °C |
12900 psi @Temperature 75.0 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, T-700 24K Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Shear Strength | 88.9 MPa @Temperature 21.1 °C |
12900 psi @Temperature 70.0 °F |
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 88.9 MPa @Temperature 177 °C |
12900 psi @Temperature 351 °F |
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64% |
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel |