Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 86.9 MPa

@Temperature 23.0 °C
12600 psi

@Temperature 73.4 °F
Hexcel® F515 Epoxy Resin, TXX200 Carbon Tape
STD MOD FiberInformation provided by HexCel
Shear Strength 86.9 MPa

@Temperature 23.0 °C
12600 psi

@Temperature 73.4 °F
Hexcel® HexPly® F515 Epoxy Resin, BXX120 Carbon Tape
Information provided by HexCel