Mechanical Properties Metric English Comments
Shear Strength 12.45 MPa

@Temperature 23.0 °C
1805 psi

@Temperature 73.4 °F
Overlap, PVC
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Shear Strength 12.45 MPa

@Time 605000 sec
1805 psi

@Time 168 hour
Overlap, PVC
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Shear Strength 12.45 MPa

@Time 3600 sec
1805 psi

@Time 1.00 hour
Overlap, Maple conditioned for 7 days AT RT/50% RH
3M Scotch-Weld™ EZ250120 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w..