Polymer Property : Shear Strength = 12.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 12.4 MPa

@Temperature 93.3 °C
1800 psi

@Temperature 200 °F
ASTM D732
Greene Tweed Avalon® 69 PTFE, Thermoplastic and Carbon Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..