Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 11.4 MPa @Temperature 149 °C |
1650 psi @Temperature 300 °F |
ASTM D732 |
Greene Tweed Avalon® 69 PTFE, Thermoplastic and Carbon Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Shear Strength | 11.4 MPa @Temperature 149 °C |
1650 psi @Temperature 300 °F |
ASTM D732 |
Greene Tweed Avalon® 7 PTFE, Pigmented and Molybdenum Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Shear Strength | 11.4 MPa @Temperature 80.0 °C |
1650 psi @Temperature 176 °F |
Double Lap Shear; Dry; 30 min @ 150°C; Hexcel IS202 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |
|||
Shear Strength | 11.4 MPa @Temperature 23.0 °C |
1650 psi @Temperature 73.4 °F |
Overlap, Maple |
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Shear Strength | 11.4 MPa @Time 3600 sec |
1650 psi @Time 1.00 hour |
Overlap, Maple conditioned for 7 days AT RT/50% RH |
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Shear Strength | 11.4 MPa @Time 605000 sec |
1650 psi @Time 168 hour |
Overlap, Maple conditioned for 7 days AT RT/50% RH |
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Shear Strength | 11.4 MPa @Temperature -40.0 °C |
1660 psi @Temperature -40.0 °F |
Overlap, FRP, Substrate Failure |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 11.4 MPa @Temperature -40.0 °C |
1660 psi @Temperature -40.0 °F |
Overlap, FRP, Substrate Failure |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 11.4 MPa @Temperature -40.0 °C |
1660 psi @Temperature -40.0 °F |
Overlap, FRP, Substrate Failure |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 11.4 MPa @Temperature 23.0 °C |
1650 psi @Temperature 73.4 °F |
Overlap, Maple |
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |