Polymer Property : Shear Strength = 10.8 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.0748 MPa

@Shear Rate 500 1/s,
Temperature 280 °C
10.8 psi

@Shear Rate 500 1/s,
Temperature 536 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers