Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.17 MPa @Time 7200 sec |
170 psi @Time 2.00 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 25°C at 50% RH Aged; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |