Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.129 MPa @Shear Rate 5000 1/s, Temperature 250 °C |
163.7 psi @Shear Rate 5000 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |