Polymer Property : Shear Strength = 0.241 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.241 MPa

@Temperature 107 °C
35.0 psi

@Temperature 225 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Shear Strength 0.241 MPa

@Temperature 107 °C
35.0 psi

@Temperature 225 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..