Mechanical Properties Metric English Comments
Shear Strength 0.2305 MPa

@Shear Rate 500 1/s,
Temperature 190 °C
33.43 psi

@Shear Rate 500 1/s,
Temperature 374 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers