Polymer Property : Shear Strength = 0.2041 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.001407 MPa

@Shear Rate 10.0 1/s,
Temperature 290 °C
0.2041 psi

@Shear Rate 10.0 1/s,
Temperature 554 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers