Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.2001 MPa @Shear Rate 50.0 1/s, Temperature 240 °C |
29.02 psi @Shear Rate 50.0 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |