Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 64.7 MPa @Temperature 260 °C |
9380 psi @Temperature 500 °F |
ASTM D790 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Machined Parts High abrasion resistance, very low friction coefficient property, suitable for being applied to spin component of spin apparatusInformation provided by Daelim H&L |