Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 8.96 MPa @Strain 10.0 % |
1300 psi @Strain 10.0 % |
Load Applied Parallel to Fiber Plane, Strain = load deformation in mils for sample 0.5" * 0.5" * 4" |
Zircar Ceramics ZAL-45 Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Flexural Strength | 8.96 MPa @Strain 15.0 % |
1300 psi @Strain 15.0 % |
Load Applied Normal to Fiber Plane, Strain = load deformation in mils for sample 0.5" * 0.5" * 4" |
Zircar Ceramics ZAL-45 Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |